特性級別 | 標(biāo)準(zhǔn)級||| |
牌號 | AY564 |
加工級別 | 注墮級||| |
品名 | PP AY564 新加坡聚烯烴 |
廠家(產(chǎn)地) | 新加坡聚烯烴 |
用途級別 | 通用級|||板材級||| |
PP AY564
PP AY564 聚烯烴
聚丙烯共聚物
TPC, The Polyolefin Company (Singapore) Pte Ltd
產(chǎn)品說明
COSMOPLENE AY564 is high impact PP copolymer manufactured by gas phase process technology licensed from Sumitomo Chemical Co. Japan.
COSMOPLENE AY564 is medium flow, high stiffness, high impact copolymer grade which can perform faster injection cycle.
COSMOPLENE AY564 is specially designed for tub of washing machine and electrical appliances which require high flow and high impact strength.
PP AY564
PP AY564 聚烯烴
用途 |
|
加工方法 |
|
黃卡文件號 |
|
物理性能 | 額定值 | 單位制 | 測試方法 |
---|---|---|---|
比重 | 0.900 | g/cm3 | ASTM D792 |
熔流率(熔體流動速率) | 16 | g/10 min | ASTM D1238 |
收縮率 | 內(nèi)部方法 | ||
流動:2.00 mm | 1.6 | % | |
橫向流動:2.00 mm | 1.7 | % | |
硬度 | 額定值 | 單位制 | 測試方法 |
洛氏硬度(R 級) | 92 | ASTM D785 |
機械性能 | 額定值 | 單位制 | 測試方法 |
---|---|---|---|
抗張強度 | ASTM D638 | ||
屈服 | 28.0 | MPa | |
斷裂 | 20.0 | MPa | |
伸長率(斷裂) | 200 | % | ASTM D638 |
彎曲模量 | 1320 | MPa | ASTM D790 |
沖擊性能 | 額定值 | 單位制 | 測試方法 |
懸壁梁缺口沖擊強度 | ASTM D256 | ||
-20°C | 42 | J/m | |
23°C | 80 | J/m |
熱性能 | 額定值 | 單位制 | 測試方法 |
---|---|---|---|
載荷下熱變形溫度(0.45 MPa, 未退火) | 124 | °C | ASTM D648 |
可燃性 | 額定值 | 測試方法 | |
---|---|---|---|
UL 阻燃等級 | HB | UL 94 |
注射 | 額定值 | 單位制 | |
---|---|---|---|
料筒后部溫度 | 190 到 230 | °C | |
料筒中部溫度 | 190 到 230 | °C | |
料筒前部溫度 | 190 到 230 | °C | |
模具溫度 | 30.0 | °C | |
注塑壓力 | 6.86 | MPa | |
鎖模力 | 0.98 | kN/cm2 |
PP AY564